MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM® 7642 PEI, Unfilled


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.

Physical PropertiesMetricEnglishComments
Density1.36 g/cc0.0491 lb/in³ ASTM D792
Linear Mold Shrinkage0.0025 - 0.0045 cm/cm0.0025 - 0.0045 in/in at 3.2 mm.

Mechanical Properties
Tensile Strength, Ultimate152 MPa22000 psi ASTM D638
Elongation at Break2 %2 % ASTM D638
Flexural Modulus8.957 GPa1300 ksi ASTM D790
Izod Impact, Notched0.53 J/cm0.993 ft-lb/in 23°C (73.4°F)

Electrical Properties
Surface Resistance1e+007 ohm1e+007 ohm 

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)210 °C410 °F ASTM D648

Processing Properties
Processing Temperature354 - 376 °C669 - 709 °F melt temperature
Mold Temperature135 - 162 °C275 - 324 °F 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.