MatWeb, The Online Materials Database

SABIC Innovative Plastics ULTEM® FULC20 PEI, Unfilled


Subcategory: Polyetherimide; Polymer; Thermoplastic

Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.

Material Notes:
Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.

Physical PropertiesOriginal ValueComments
Density1.3 g/cc Typical Value for PEI

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.