SABIC Innovative Plastics VALOX® 830U PBT, 30% Glass Filler
Subcategory: Filled/Reinforced Thermoplastic; Polybutylene Terephthalate (PBT); Polyester, TP; Polymer; Thermoplastic
Close Analogs: Saudi Basic Industries Corporation (SABIC) announced on August 31st, 2007, the completion of its purchase of GE Plastics.
Material Notes: Data provided by GE Plastics. This product grade was removed from GE's database of standard products in 1998.
Physical Properties | Metric | English | Comments |
|
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
Water Absorption | 0.06 % | 0.06 % | 24 hrs at 23°C; ASTM D570 |
Linear Mold Shrinkage | 0.005 - 0.008 cm/cm | 0.005 - 0.008 in/in | at 6.4 mm. |
Linear Mold Shrinkage | 0.003 - 0.008 cm/cm | 0.003 - 0.008 in/in | at 3.2 mm. |
Mechanical Properties |
|
Tensile Strength, Ultimate | 107 MPa | 15500 psi | ASTM D638 |
Flexural Modulus | 6.89 GPa | 999 ksi | ASTM D790 |
Izod Impact, Notched | 0.8 J/cm | 1.5 ft-lb/in | 23°C (73.4°F) |
Electrical Properties |
|
Electrical Resistivity | 4e+016 ohm-cm | 4e+016 ohm-cm | ASTM D257 |
Dielectric Constant | 3.5 | 3.5 | at 1MHz |
Dissipation Factor | 0.02 | 0.02 | at 1 MHz |
Thermal Properties |
|
CTE, linear 20°C | 25 µm/m-°C | 13.9 µin/in-°F | |
Deflection Temperature at 0.46 MPa (66 psi) | 221 °C | 430 °F | ASTM D648 |
Deflection Temperature at 1.8 MPa (264 psi) | 193 °C | 379 °F | ASTM D648 |
UL RTI, Electrical | 120 °C | 248 °F | |
UL RTI, Mechanical without Impact | 120 °C | 248 °F | |
Flammability, UL94 | HB | HB | 1.6 mm |
Processing Properties |
|
Processing Temperature | 243 - 265 °C | 469 - 509 °F | melt temperature |
Mold Temperature | 65 - 87 °C | 149 - 189 °F | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|