Gharda Chemicals GAFONE™ 3300 PES, High Viscosity Grade


Subcategory: Polyethersulfone; Polymer; Thermoplastic

Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.

Material Notes:
Unreinforced high viscosity grade for injection molding, extrusion molding, blow molding, calendering, etc.

Characteristics:

  • Very high rigidity
  • Good dielectric properties
  • High mechanical strength
  • Good dimensional stability
  • Good resistance to hydrolysis and sterilization
  • Good oxidative stability
  • Inherent flame retardance

Applications:

  • Reusable hypodermic syringes
  • Surgical instruments and components
  • Printed circuit boards
  • Circuit breaker components
  • Oil level indicators
  • Heat exchanger parts
  • Engine components
  • Household appliances
  • Filter housings
  • Sanitary and pipe fittings

Information provided by Gharda.

Physical PropertiesOriginal ValueComments
Density1.37 g/cc ISO 1183
Moisture Absorption at Equilibrium0.4 % ISO 62
Linear Mold Shrinkage0.005 cm/cm ASTM D955
Melt Flow26 - 40 g/10 min 380°C, 2.16 kg, 6 mins; ASTM D1238

Mechanical Properties
Tensile Strength at Break90 MPa ISO 527
Elongation at Break6 % ISO 527
Tensile Modulus2.8 GPa ISO 527
Flexural Modulus2.6 GPa ISO 178
Flexural Strength120 MPa ISO 178
Izod Impact, Notched (ISO)5 kJ/m˛ ISO 180/1A

Electrical Properties
Volume ResistivityMin 1e+016 ohm-cm IEC 93
Surface ResistanceMin 1e+014 ohm IEC 93
Dielectric Strength16 kV/mm IEC 243/1
Arc Resistance80 sec ASTM D495
Comparative Tracking Index150 V IEC 112

Thermal Properties
Maximum Service Temperature, Air185 °C Continuous use
Deflection Temperature at 1.8 MPa (264 psi)205 °C ISO 75
Glass Temperature225 °C DSC
Flammability, UL94V-0 
Oxygen Index38 % ISO 4589

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.