MatWeb, The Online Materials Database
Gharda Chemicals GAFONE™ 3500 PES, Unreinforced, Easy Flow
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes: Easy flow unreinforced grade for injection molding of thin walled components Characteristics: - Very high rigidity
- Good dielectric properties
- High mechanical strength
- Good dimensional stability
- Good resistance to hydrolysis and sterilization
- Good oxidative stability
- Inherent flame retardance
Applications: - Reusable hypodermic syringes
- Surgical instruments and components
- Printed circuit boards
- Circuit breaker components
- Oil level indicators
- Heat exchanger parts
- Engine components
- Household appliances
- Filter housings
- Sanitary and pipe fittings
Information provided by Gharda.
| Physical Properties | Original Value | Comments |
|
| Density | 1.37 g/cc | ISO 1183 |
| Moisture Absorption at Equilibrium | 0.4 % | ISO 62 |
| Linear Mold Shrinkage | 0.005 cm/cm | ASTM D955 |
| Melt Flow | 51 - 70 g/10 min | 380°C, 2.16 kg, 6 mins; ASTM D1238 |
Mechanical Properties |
|
| Tensile Strength at Break | 90 MPa | ISO 527 |
| Elongation at Break | 6 % | ISO 527 |
| Tensile Modulus | 2.8 GPa | ISO 527 |
| Flexural Modulus | 2.6 GPa | ISO 178 |
| Flexural Strength | 120 MPa | ISO 178 |
| Izod Impact, Notched (ISO) | 5 kJ/m˛ | ISO 180/1A |
Electrical Properties |
|
| Volume Resistivity | Min 1e+016 ohm-cm | IEC 93 |
| Surface Resistance | Min 1e+014 ohm | IEC 93 |
| Dielectric Strength | 16 kV/mm | IEC 243/1 |
| Arc Resistance | 80 sec | ASTM D495 |
| Comparative Tracking Index | 150 V | IEC 112 |
Thermal Properties |
|
| Maximum Service Temperature, Air | 185 °C | Continuous use |
| Deflection Temperature at 1.8 MPa (264 psi) | 205 °C | ISO 75 |
| Glass Temperature | 225 °C | DSC |
| Flammability, UL94 | V-0 | |
| Oxygen Index | 38 % | ISO 4589 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |