MatWeb, The Online Materials Database

Gharda Chemicals GAFONE™ 3200 PES, High Viscosity Grade


Subcategory: Filled/Reinforced Thermoplastic; Polyethersulfone; Polymer; Thermoplastic

Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.

Material Notes:
High viscosity grade for membrane and coating applications.

Characteristics:

  • Very high rigidity
  • Good dielectric properties
  • High mechanical strength
  • Good dimensional stability
  • Good resistance to hydrolysis and sterilization
  • Good oxidative stability
  • Inherent flame retardance

Applications:

  • Reusable hypodermic syringes
  • Surgical instruments and components
  • Printed circuit boards
  • Circuit breaker components
  • Oil level indicators
  • Heat exchanger parts
  • Engine components
  • Household appliances
  • Filter housings
  • Sanitary and pipe fittings

Information provided by Gharda.

Physical PropertiesOriginal ValueComments
Melt Flow20 - 25 g/10 min 380°C, 2.16 kg, 6 mins; ASTM D1238

Thermal Properties
Maximum Service Temperature, Air210 °C Temperature resistance

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.