MatWeb, The Online Materials Database
Gharda Chemicals Gafone™ 3000P Polyethersulfone (PES)
Subcategory: Polyethersulfone; Polymer; Thermoplastic
Close Analogs: Solvay Advanced Polymers completed its acquisition of Gharda Polymers Division in May 2006. Current product data sheets are available under the Solvay Advanced Polymers name.
Material Notes:
Characteristics: - Excellent Thermal Resistance - Tg 224°C
- Outstanding Mechanical, Electrical, Flame & Chemical Resistance
- Very good Hydrolytic & Sterilization Resistance
- Good Optical Clarity
- Processed by all Conventional Techniques
Applications: - Clear applications like baby bottle, snuffer buttons, tee lights etc.
- Membrane applications
- Industrial and domestic coating
- Medical - Sterilizable box, surgical instrument
- Automotive - engine components
- Household - microwave oven food trays
- Industrial - oil level indicator, high temp. lighting fixture, Heat exchanger parts
- Electrical - Printed circuit board
Information provided by Gharda Chemicals
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.37 g/cc | 0.0495 lb/in³ | ASTM D792 |
| Volatiles | 0.5 % | 0.5 % | P/QA/I/306 |
| Viscosity | 6500 cP | 6500 cP | Viscosity of 25%(w/w) Solution in NMP @ 25°C; P/QA/I/326 |
| Viscosity Test | 0.28 cm³/g | 0.28 cm³/g | Intrinsic Viscosity in DMF @ 25°C; ASTM 2857 |
| Molecular Weight | 160000 g/mol | 160000 g/mol | P/QA/I/314 |
Chemical Properties |
|
| Ionic Impurities - Cl (Chloride) | 100 ppm | 100 ppm | P/QA/I/304 |
Mechanical Properties |
|
| Tensile Strength, Yield | 90 MPa | 13100 psi | ASTM D638 |
| Elongation at Break | 25 - 75 % | 25 - 75 % | ASTM D638 |
| Tensile Modulus | 2.5 GPa | 363 ksi | ASTM D638 |
| Flexural Modulus | 2.5 GPa | 363 ksi | ASTM D790 |
| Flexural Strength | 115 MPa | 16700 psi | ASTM D790 |
| Izod Impact, Notched | 0.45 J/cm | 0.843 ft-lb/in | ASTM D256 |
Processing Properties |
|
| Moisture Content | 0.5 % | 0.5 % | P/QA/I/043 |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |