Physical PropertiesMetricEnglishComments
Density1.14 g/cc0.0412 lb/in³ ISO 1183
Water Absorption3 %3 % 23°C / 50% RH; ISO 62
Water Absorption at Saturation9 %9 % ISO 62
Linear Mold Shrinkage0.008 cm/cm0.008 in/in ISO 294
Linear Mold Shrinkage, Transverse0.0095 cm/cm0.0095 in/in ISO 294

Mechanical Properties
Hardness, Shore D140140 ISO 868
Tensile Strength at Break70 MPa10200 psi 50 mm/min; ISO 527
Elongation at Break5 %5 % 50 mm/min; ISO 527
Tensile Modulus3.3 GPa479 ksi 1 mm/min; ISO 527
Charpy Impact UnnotchedMin 10 J/cm²Min 47.6 ft-lb/in² ISO 179/1eU
Charpy Impact, Notched, Low Temp0.4 J/cm²1.9 ft-lb/in²  -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low TempMin 10 J/cm²Min 47.6 ft-lb/in²  -30°C; ISO 179/1eU
Charpy Impact, Notched0.4 J/cm²1.9 ft-lb/in² ISO 179/1eA

Electrical Properties
Volume Resistivity1e+014 ohm-cm1e+014 ohm-cm IEC 60093
Dielectric Strength30 kV/mm762 kV/in IEC 60243-1

Thermal Properties
CTE, linear 20°C100 µm/m-°C55.6 µin/in-°F trans. (23-55°C); ISO 11359
CTE, linear 20°C70 µm/m-°C38.9 µin/in-°F long. (23-55°C); ISO 11359
Melting Point222 °C432 °F ISO 11357
Maximum Service Temperature, Air70 - 90 °C158 - 194 °F Long Term; ISO 2578
Maximum Service Temperature, Air160 °C320 °F Short Term; ISO 2578
Deflection Temperature at 0.46 MPa (66 psi)170 °C338 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)55 °C131 °F ISO 75
Flammability, UL94HBHB 0.8 mm; ISO 1210

Processing Properties
Processing Temperature80 °C176 °F Tool
Rear Barrel Temperature260 °C500 °F Zone 3
Middle Barrel Temperature255 °C491 °F Zone 2
Front Barrel Temperature250 °C482 °F Zone 1
Nozzle Temperature260 °C500 °F 
Melt Temperature240 - 300 °C464 - 572 °F Basic machine settings
Drying TemperatureMax 80 °CMax 176 °F Desiccant Dryer (dew point at -25°F)
Drying TemperatureMax 100 °CMax 212 °F Vacuum Oven
Dry Time4 - 12 hour4 - 12 hour Desiccant Dryer (dew point at -25°F)
Dry Time4 - 12 hour4 - 12 hour Vacuum Oven
Hold Pressure30 - 80 MPa4350 - 11600 psi 
Back Pressure0.5 - 1.5 MPa72.5 - 218 psi 
Screw Speed50 - 100 rpm50 - 100 rpm 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.