EMS-Grivory Grilon® FE 8023 Natural Nylon 6, Dry As Molded


Subcategory: Nylon; Nylon 6; Polymer; Thermoplastic

Material Notes:
Grilon FE 8023 natural is a new heat stabilized injection molding grade based on Polyamide 6.

Information provided by EMS-Grivory

Physical PropertiesMetricEnglishComments
Density1.15 g/cc0.0415 lb/in³ ISO 1183
Linear Mold Shrinkage0.009 cm/cm0.009 in/in ISO 294
Linear Mold Shrinkage, Transverse0.006 cm/cm0.006 in/in ISO 294
Melt Flow57.5 g/10 min57.5 g/10 min 275°C / 5kg; ISO 11133

Mechanical Properties
Tensile Strength at Break100 MPa14500 psi 5 mm/min; ISO 527
Elongation at Break3 %3 % 5 mm/min; ISO 527
Tensile Modulus4.6 GPa667 ksi 1 mm/min; ISO 527
Charpy Impact Unnotched7 J/cm²33.3 ft-lb/in² ISO 179/1eU
Charpy Impact, Notched, Low Temp0.4 J/cm²1.9 ft-lb/in²  -30°C; ISO 179/1eA
Charpy Impact, Unnotched Low Temp6.5 J/cm²30.9 ft-lb/in²  -30°C; ISO 179/1eU
Charpy Impact, Notched0.4 J/cm²1.9 ft-lb/in² ISO 179/1eA

Thermal Properties
Melting Point220 °C428 °F ISO 11357
Deflection Temperature at 0.46 MPa (66 psi)180 °C356 °F ISO 75
Deflection Temperature at 1.8 MPa (264 psi)100 °C212 °F ISO 75

Processing Properties
Melt Temperature240 - 300 °C464 - 572 °F Injection molding
Mold Temperature80 - 100 °C176 - 212 °F Injection molding
Hold Pressure50 - 75 MPa7250 - 10900 psi 
Back Pressure0.5 - 1.5 MPa72.5 - 218 psi 
Screw Speed50 - 100 rpm50 - 100 rpm 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.