MatWeb, The Online Materials Database
EMS-Grivory Grilon® XS 1306.1 Nylon 610, Dry As Molded
Subcategory: Nylon; Nylon 610; Polymer; Thermoplastic
Material Notes: Grilon XS 1306.1 is a medium viscosity, nylon 6.10 homopolymer. It is particularly well-suited for monofilaments. Grilon XS 1306.1 exhibits excellent strength, toughness, ductility, heat stability and abrasion resistance. Grilon XS 1306.1 also offers very good resistance to a wide range of chemicals, solvents, oils and greases.Information provided by EMS-Grivory
| Physical Properties | Original Value | Comments |
|
| Density | 1.08 g/cc | ASTM D792 |
| Water Absorption | 0.46 % | 24 hr immersion; ASTM D570 |
Mechanical Properties |
|
| Hardness, Shore D | 81 | |
| Tensile Strength at Break | 61 MPa | ASTM D638 |
| Elongation at Break | 30 % | ASTM D638 |
| Flexural Modulus | 2.145 GPa | ASTM D790 |
| Flexural Strength | 90 MPa | ASTM D790 |
| Izod Impact, Notched | 0.8 ft-lb/in | ASTM D256 |
Thermal Properties |
|
| Melting Point | 222 °C | DSC |
| Deflection Temperature at 0.46 MPa (66 psi) | 136 °C | ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 53 °C | ASTM D648 |
Processing Properties |
|
| Rear Barrel Temperature | 232 °C | Extrusion |
| Rear Barrel Temperature | 245 °C | Injection Molding |
| Middle Barrel Temperature | 232 °C | Extrusion |
| Middle Barrel Temperature | 255 °C | Injection Molding |
| Front Barrel Temperature | 227 °C | Extrusion |
| Front Barrel Temperature | 265 °C | Injection Molding |
| Nozzle Temperature | 255 °C | Injection Molding |
| Die Temperature | 450 °F | Extrusion |
| Melt Temperature | 233 °C | Extrusion |
| Melt Temperature | 265 °C | Injection Molding |
| Mold Temperature | 60 °C | Injection Molding |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |