EMS-Grivory Grilon® XS 1392 Nylon Copolymer


Subcategory: Nylon; Nylon 610; Polymer; Thermoplastic

Material Notes:
Grilon XS 1392 is a special heat stabilized and modified co polyamide especially developed for high performance sealing layers.

Grilon XS 1392 is very well suited as a sealing layer in “cook in bag” and any other mechanically demanded heat sealed application.

Information provided by EMS-Grivory

Physical PropertiesOriginal ValueComments
Density1.02 g/cc ISO 1183
Water Absorption1.5 % 23°C / 50% RH; ISO 62
Water Absorption at Saturation3.5 % ISO 62
Water Vapor Transmission10 g/m²/day 23°C / 85% RH; DIS/ISO 15106-1
Oxygen Transmission10.1 cc-mm/m²-24hr-atm 23°C / 85% RH; DIS/ISO 15105-1
Oxygen Transmission15.2 cc-mm/m²-24hr-atm 23°C / 0% RH; DIS/ISO 15105-1
Carbon Dioxide Transmission60.8 cc-mm/m²-24hr-atm 23°C / 85% RH; DIS/ISO 15105-2
Carbon Dioxide Transmission60.8 cc-mm/m²-24hr-atm 23°C / 0% RH; DIS/ISO 15105-2
Melt Flow163 g/10 min 275°C / 5kg; ISO 1133

Mechanical Properties
Tensile Strength at Break70 MPa normal; ISO 527-3
Film Tensile Strength at Yield, MD33 MPa ISO 527-3
Film Tensile Strength at Break, MD75 MPa ISO 527-3
Film Elongation at Break, MD800 % ISO 527-3
Film Elongation at Yield, MD8 % ISO 527-3
Tensile Strength, Yield30 MPa normal; ISO 527-3
Elongation at Break800 % normal; ISO 527-3
Elongation at Yield7 % normal; ISO 527-3
Tensile Modulus0.8 GPa 4 mm bar; ISO 527-2
Tear Strength Test50 [N/mm]; ISO 6383-1

Thermal Properties
Melting Point178 °C ISO 11357

Optical Properties
Gloss60 % 60°; ISO 2813

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.