MatWeb, The Online Materials Database
EMS-Grivory Grilon® XS 1423 Natural Nylon 6, Dry As Molded
Subcategory: Nylon; Nylon 6; Polymer; Thermoplastic
Material Notes: Grilon XS1423 Natural is a heat stabilized, high viscosity, impact modified and plasticized PA6 extrusion grade. Grilon XS1423 Natural is used typically for co-extruded fuel lines, coolant pipes in deep freezer units, vulcanization mandrels, and vacuum lines. Information provided by EMS-Grivory
| Physical Properties | Metric | English | Comments |
|
| Density | 1.08 g/cc | 0.039 lb/in³ | ASTM D792 |
| Melt Flow | 18.4 g/10 min | 18.4 g/10 min | 275°C / 5kg; ASTM D1238 |
Mechanical Properties |
|
| Tensile Strength at Break | 54.3 MPa | 7880 psi | 50 mm/min; ASTM D638 |
| Elongation at Break | 41 % | 41 % | 50 mm/min; ASTM D638 |
| Flexural Modulus | 0.348 GPa | 50.5 ksi | 2 mm/min; ASTM D790 |
Processing Properties |
|
| Processing Temperature | 230 - 260 °C | 446 - 500 °F | Metering zone |
| Processing Temperature | 230 - 260 °C | 446 - 500 °F | Compression zone |
| Feed Temperature | 190 - 250 °C | 374 - 482 °F | |
| Nozzle Temperature | 230 - 260 °C | 446 - 500 °F | |
| Melt Temperature | 230 - 260 °C | 446 - 500 °F | Basic Machine Settings |
| Head Temperature | 230 - 260 °C | 446 - 500 °F | |
| Drying Temperature | Max 100 °C | Max 212 °F | Vacuum Oven |
| Drying Temperature | Max 80 °C | Max 176 °F | Desiccant Dryer (dew point at -30°C) |
| Dry Time | 4 - 12 hour | 4 - 12 hour | Desiccant Dryer (dew point at -30°C) |
| Dry Time | 4 - 12 hour | 4 - 12 hour | Vacuum Oven |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |