MatWeb, The Online Materials Database
PolyOne Stat-Tech™ PI-05CF/000 EM Polyetherimide (PEI)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Material Notes: Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low-to-high levels of conductivity depending upon application requirements.Description/Features: - PEI (Polyetherimide)
- 5% Carbon Fiber Reinforced
- ESD Protection
- Antistatic
- Static Dissipative
Applications: - EMI?RFI Shielding
- Printer Components
- Enclosures
- Fuel Systems
Processing Method: Injection Molding Information provided by PolyOne Corporation
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.29 g/cc | ASTM D792 |
| Water Absorption | 0.25 % | 24 hr. Immersion, 0.125 in; ASTM D570 |
| Linear Mold Shrinkage | 0.004 - 0.006 cm/cm | ASTM D955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 18000 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
| Elongation at Break | 4 - 5 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 650000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 650000 psi | ASTM D790 |
| Flexural Strength | 28000 psi | ASTM D790 |
| Izod Impact, Notched | 0.9 ft-lb/in | Method A, Injection Molded, 0.250 in bars, 73°F(23°C); ASTM D256 |
Electrical Properties |
|
| Volume Resistivity | 1000 - 100000 ohm-cm | ASTM D257 |
| Surface Resistivity per Square | 1000 - 100000 ohm | ASTM D257 |
Thermal Properties |
|
| Deflection Temperature at 0.46 MPa (66 psi) | 405 °F | Unannealed; ASTM D648 |
| Deflection Temperature at 1.8 MPa (264 psi) | 390 °F | Unannealed; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 670 - 720 °F | Molding |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |