MatWeb, The Online Materials Database
PolyOne Edgetek® PI-1000 Polyetherimide (PEI)
Subcategory: Polyetherimide; Polymer; Thermoplastic
Material Notes: The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Description/Features: - PEI (Polyetherimide)
- Unfilled
- Hi-Temp
Applications: Multi-purpose Processing Method: Injection Molding Information provided by PolyOne Corporation
| Physical Properties | Metric | English | Comments |
|
| Specific Gravity | 1.27 g/cc | 0.0459 lb/in³ | ASTM D792 |
| Water Absorption | 0.25 % | 0.25 % | 24 hr. Immersion, 0.125 in; ASTM D570 |
| Linear Mold Shrinkage | 0.007 - 0.009 cm/cm | 0.007 - 0.009 in/in | ASTM D955 |
Mechanical Properties |
|
| Tensile Strength @ Yield | 105 MPa | 15200 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
| Elongation at Break | 7 - 8 % | 7 - 8 % | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 2.96 GPa | 430 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 2.9 GPa | 420 ksi | ASTM D790 |
| Flexural Strength | 152 MPa | 22000 psi | ASTM D790 |
| Izod Impact, Notched | 0.534 J/cm | 1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F(23°C); ASTM D256 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 200 °C | 392 °F | Unannealed; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 327 - 371 °C | 620 - 700 °F | Molding |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of