MatWeb, The Online Materials Database

PolyOne Geon® 1351 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Enhanced Heat Stability
  • High Flow

Applications:

  • General Purpose
  • Fence Wire Coating

Processing Method:

  • Extrusion

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.32 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D63 15 sec; ASTM D2240
Tensile Strength, Ultimate3000 psi 20 in/min, 100% in/in; ASTM D638
Tensile Strength, Ultimate3150 psi 20 in/min; ASTM D638
Elongation at Break170 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Brittleness Temperature32 °F ASTM D746

Processing Properties
Melt Temperature345 - 355 °F Extrusion

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.