MatWeb, The Online Materials Database

PolyOne Geon® 1410XX8OFRD Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

UL 105 C wire & cable insulation compound. THHN,THWN,THW,MTW,UL STYLES 1015,1007 and NMB insulation.
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.39 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A91 15 sec; ASTM D2240
Tensile Strength, Yield3100 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break280 % Type 4 - Flexibles, 20 in/min; ASTM D638

Electrical Properties
Volume Resistivity1e+015 ohm-cm ASTM D257

Thermal Properties
Brittleness Temperature-12 °F ASTM D746
Oxygen Index31.7 % 0.075 in; ASTM D2863

Processing Properties
Melt Temperature350 - 365 °F Extrusion

Descriptive Properties
Oven Aged - Retention of Elongation (ROE)95 % 277°F (136°C), 168 hrs (7 days), 0.020 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)80 % 277°F (136°C), 168 hrs (7 days), 0.020 in; UL Standard

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.