  • Packaging

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Density0.801 g/cc0.0289 lb/in³ ASTM D1505
Specific Gravity1.32 g/cc0.0477 lb/in³ ASTM D792

Mechanical Properties
Hardness, Rockwell R105105 ASTM D785
Hardness, Shore D8080 Instantaneous; ASTM D2240
Tensile Strength, Yield44.8 MPa6500 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.3 GPa334 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.65 GPa384 ksi ASTM D790
Flexural Strength83.4 MPa12100 psi ASTM D790
Izod Impact, Notched10.6 J/cm19.9 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)66.1 °C151 °F Unannealed, 0.125 in bars; ASTM D648

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.