MatWeb, The Online Materials Database
PolyOne Geon® 161JA White Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - High Impact
- High Gloss
- Opaque
- Interior
Applications: Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
Specific Gravity | 1.35 g/cc | 0.0488 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 80 | 80 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 43.1 MPa | 6250 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Tensile Modulus | 2.32 GPa | 336 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.68 GPa | 388 ksi | ASTM D790 |
Flexural Strength | 73.8 MPa | 10700 psi | ASTM D790 |
Izod Impact, Notched | 10.8 J/cm | 20.2 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 66.7 °C | 152 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|