PolyOne Geon® 1699 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • High Impact
  • High Gloss

Applications:

  • General Purpose
  • Multi-Purpose
  • Bottles

Market:

  • Packaging
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Density0.801 g/cc0.0289 lb/in³ ASTM D1505
Specific Gravity1.32 g/cc0.0477 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D7979 Instantaneous; ASTM D2240
Tensile Strength, Yield42.1 MPa6100 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.24 GPa325.5 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.45 GPa356 ksi ASTM D790
Flexural Strength65.8 MPa9550 psi ASTM D790
Izod Impact, Notched11.3 J/cm21.2 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)59.4 °C139 °F Unannealed, 0.125 in bars; ASTM D648

Optical Properties
Transmission, Visible38.5 %38.5 % 30.0 mils, 700 nm
Transmission, Visible7.5 %7.5 % 30.0 mils, 400 nm

Processing Properties
Melt Temperature196 - 210 °C385 - 410 °F Blow Molding

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.