MatWeb, The Online Materials Database
PolyOne Geon® 1699 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: - General Purpose
- Multi-Purpose
- Bottles
Market: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Density | 50 lb/ft³ | ASTM D1505 |
Specific Gravity | 1.32 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 79 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 6100 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 325500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 356 ksi | ASTM D790 |
Flexural Strength | 9550 psi | ASTM D790 |
Izod Impact, Notched | 21.2 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 139 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 38.5 % | 30.0 mils, 700 nm |
Transmission, Visible | 7.5 % | 30.0 mils, 400 nm |
Processing Properties |
|
Melt Temperature | 385 - 410 °F | Blow Molding |
Descriptive Properties | |
Product Form | Pellets | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|