MatWeb, The Online Materials Database

PolyOne Geon® 1725-xx13FRD Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL Recognized 300 hr. Sunlight Resistant Jacket per UL QMTT2
  • UL 60°C
  • UL 719 NMC Jacket
  • UL 854 UF Jacket
  • TW
  • Flame Retardant

Applications:

  • General Purpose
  • Building Wire Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.38 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A78 15 sec; ASTM D2240
Tensile Strength, Yield2100 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break300 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Brittleness Temperature-14.8 °F ASTM D746
Oxygen Index27 % 0.075 in; ASTM D2863

Processing Properties
Melt Temperature335 °F Extrusion

Descriptive Properties
Oven Aged - Retention of Elongation (ROE)85 % 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)100 % 212°F (100°C), 168 hrs (7 days), 0.075 in; UL Standard
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.