MatWeb, The Online Materials Database
PolyOne Geon® 1740-xx51FRD Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL Recognized Insulation per UL QMTT2
- TW
- UL 75°C
- Good Low Temperature Impact
- Flame Retardant
Applications: - Building Wire Insulation
- Power and Control Cable Insulation
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.33 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 80 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 2800 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 330 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Electrical Properties |
|
Volume Resistivity | 5e+013 ohm-cm | ASTM D257 |
Thermal Properties |
|
Brittleness Temperature | -20.2 °F | ASTM D746 |
Oxygen Index | 27 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
Melt Temperature | 335 - 350 °F | Extrusion |
Descriptive Properties | |
Oven Aged - Retention of Elongation (ROE) | 85 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Oven Aged - Retention of Tensile Strength (ROT) | 100 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Product Form | Pellets/Cubes | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|