MatWeb, The Online Materials Database

PolyOne Geon® 1741-xx06D Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL 75°C
  • SAE J-1128 Automotive Application

Applications:

  • Automotive Insulation

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.33 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A87 15 sec; ASTM D2240
Tensile Strength, Yield2900 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break280 % Type 4 - Flexibles, 20 in/min; ASTM D638

Electrical Properties
Volume Resistivity2e+012 ohm-cm ASTM D257

Processing Properties
Melt Temperature345 - 360 °F Extrusion

Descriptive Properties
Oven Aged - Retention of Elongation (ROE)100 % 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)85 % 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.