MatWeb, The Online Materials Database

PolyOne Geon® 1802-xx11FRD Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL Recognized 720 hr. Sunlight Resistant Jacket per UL QMTT2
  • PLTC
  • UL 105°C
  • Flame Retardant

Applications:

  • Power and Control Cable Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.42 g/cc0.0513 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8585 15 sec; ASTM D2240
Tensile Strength, Yield17.9 MPa2600 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break300 %300 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Brittleness Temperature-19 °C-2.2 °F ASTM D746
Oxygen Index29 %29 % 0.075 in; ASTM D2863

Processing Properties
Melt Temperature171 - 179 °C340 - 355 °F Extrusion

Descriptive Properties
Oven Aged - Retention of Elongation (ROE)99 % 277°F (136°C), 168 hrs (7 days), 0.075 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)87 % 277°F (136°C), 168 hrs (7 days), 0.075 in; UL Standard
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.