MatWeb, The Online Materials Database

PolyOne Geon® 2020 LO-GC Vinyl Compound - Rigid (RPVC)


Subcategory: Filled/Reinforced Thermoplastic; Polymer; Thermoplastic; Vinyl

Material Notes:

Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor applications that require FDA sanctioned materials.

Description/Features:

  • Transparent
  • High Impact
  • High Gloss
  • Low taste and odor

Applications:

  • FDA (Food Contact)
  • Bottles

Market:

  • Packaging

Processing Method:

  • Blow Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Density50 lb/ft³ ASTM D1505
Specific Gravity1.32 g/cc ASTM D792

Mechanical Properties
Hardness, Rockwell R105 ASTM D785
Hardness, Shore D79 Instantaneous; ASTM D2240
Tensile Strength, Yield6630 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus342000 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus395 ksi ASTM D790
Flexural Strength11600 psi ASTM D790
Izod Impact, Notched19.4 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)143 °F Unannealed, 0.125 in bars; ASTM D648

Optical Properties
Transmission, Visible60 % 33.5 mils, 400 nm
Transmission, Visible85 % 33.5 mils, 700 nm

Processing Properties
Melt Temperature370 - 390 °F Blow Molding

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.