MatWeb, The Online Materials Database

PolyOne Geon® 210(HS) Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • NSF Type I
  • Normal Impact
  • High Flow

Market:

  • Fittings (Potable Water, DWV, etc.)

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.42 g/cc0.0513 lb/in³ ASTM D792
Linear Mold Shrinkage0.002 - 0.005 cm/cm0.002 - 0.005 in/in ASTM D955

Mechanical Properties
Hardness, Shore D8181 Instantaneous; ASTM D2240
Tensile Strength, Yield49 MPa7100 psi Type 1 - Rigids, 2 in/min; ASTM D638
Tensile Modulus2.79 GPa405 ksi Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Modulus2.79 GPa405 ksi ASTM D790
Flexural Strength93.1 MPa13500 psi ASTM D790
Izod Impact, Notched0.534 J/cm1 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)70.6 °C159 °F Unannealed, 0.250 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi)72.2 °C162 °F Annealed, 0.250 in bars; ASTM D648

Processing Properties
Melt Temperature199 - 210 °C390 - 410 °F Molding

Descriptive Properties
Cell Classification D178412454 ASTM D1784
NSFAcceptable Std 14-Plastic Piping Comp.
NSFAcceptable Std 61-Drinking Water Appl.
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.