MatWeb, The Online Materials Database

PolyOne Geon® 210A Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • NSF Type I
  • Normal Impact
  • Medium Flow

Market:

  • Fittings (Potable Water, DWV, etc.)

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.41 g/cc ASTM D792
Linear Mold Shrinkage0.002 - 0.005 cm/cm ASTM D955

Mechanical Properties
Hardness, Shore D81 Instantaneous; ASTM D2240
Tensile Strength, Yield7100 psi Type 1 - Rigids, 2 in/min; ASTM D638
Tensile Modulus410000 psi Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Modulus415 ksi ASTM D790
Flexural Strength12500 psi ASTM D790
Izod Impact, Notched2.5 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)160 °F Unannealed, 0.250 in bars; ASTM D648

Processing Properties
Melt Temperature390 - 410 °F Molding

Descriptive Properties
Cell Classification D178412454 ASTM D1784
NSFAcceptable Std 14-Plastic Piping Comp.
NSFAcceptable Std 61-Drinking Water Appl.
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.