Physical PropertiesMetricEnglishComments
Specific Gravity1.35 g/cc0.0488 lb/in³ ASTM D792
Linear Mold Shrinkage0.002 - 0.005 cm/cm0.002 - 0.005 in/in ASTM D955

Mechanical Properties
Tensile Strength, Yield43.4 MPa6300 psi Type 1 - Rigids, 2 in/min; ASTM D638
Tensile Modulus2.55 GPa370 ksi Type 1 - Rigids, 2 in/min; ASTM D638
Flexural Modulus2.62 GPa380 ksi ASTM D790
Flexural Strength82.7 MPa12000 psi ASTM D790
Izod Impact, Notched9.88 J/cm18.5 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)70.6 °C159 °F Unannealed, 0.250 in bars; ASTM D648

Processing Properties
Melt Temperature199 - 210 °C390 - 410 °F Molding

Descriptive Properties
Cell Classification D178416344 ASTM D1784
NSFAcceptable Std 14-Plastic Piping Comp.
NSFAcceptable Std 61-Drinking Water Appl.
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.