MatWeb, The Online Materials Database
PolyOne Geon® 2121C Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
A Clear Rigid PVC Compound designed specifically for water bottle applications. Description/Features: - Transparent
- High Impact
- High Gloss
Applications: - FDA (Food Contact)
- Bottles
Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Physical Properties | Metric | English | Comments |
|
| Density | 0.801 g/cc | 0.0289 lb/in³ | ASTM D1505 |
| Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Mechanical Properties |
|
| Hardness, Rockwell R | 100 | 100 | ASTM D785 |
| Hardness, Shore D | 83 | 83 | Instantaneous; ASTM D2240 |
| Tensile Strength, Yield | 41.4 MPa | 6000 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 2.72 GPa | 394 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 2.63 GPa | 382 ksi | ASTM D790 |
| Flexural Strength | 78.4 MPa | 11370 psi | ASTM D790 |
| Izod Impact, Notched | 12.4 J/cm | 23.2 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
| Deflection Temperature at 1.8 MPa (264 psi) | 65 °C | 149 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
| Transmission, Visible | 81 % | 81 % | 33.5 mils, 400 nm |
| Transmission, Visible | 86.5 % | 86.5 % | 33.5 mils, 700 nm |
Processing Properties |
|
| Melt Temperature | 199 - 213 °C | 390 - 415 °F | Blow Molding |
Descriptive Properties | |
| Product Form | Pellets | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from