MatWeb, The Online Materials Database
PolyOne Geon® 213 Polyvinyl Chloride Homopolymer (PVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Excellent non-settling qualities
- Reduces surface gloss of plastisol
- Provides Brookfield & Severs viscosity ability
- High filler loading capability
Applications: - Recommended for thin plastisol applications (4+ mils)
- General plastisol formulations
- Dip coated products
- Cast Products
- Strand Coating
Suspension Polymerization ProcessDisclaimer: Note: Plastisol Formulation F1 consists of 60 parts of 178 + 40 parts of this resin + 60 parts DOP Note: Plastisol and/or Fused Film Formulation F2 consists of 60 parts Geon 121® + 40 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent "typical" values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Manufacturing Location: This resin is produced at PolyOne Corporation's Henry, IL facility, which is ISO 9002 certified. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Shipping: This resin can be shipped in 45,000 lb bulk trucks and 180,000 lb bulk railcars. Contact PolyOne Corporation Customer Service at 866.PolyOne for bulk shipment information and availability. Information provided by PolyOne Corporation.
We're sorry, but our sources do not report any other information for this material. We are limited by the information available from our sources, which often are not as complete as we would like. Sometimes you will see this message during a MatWeb internal update, especially around 07:00 GMT Sundays.
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |