PolyOne Geon® 216A Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - NSF Type I
- Normal Impact
- Medium Flow
- Cyclic Pressure Systems
Market: - Fittings (Potable Water, DWV, etc.)
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.39 g/cc | 0.0502 lb/in³ | ASTM D792 |
Linear Mold Shrinkage | 0.002 - 0.005 cm/cm | 0.002 - 0.005 in/in | ASTM D955 |
Mechanical Properties |
|
Hardness, Shore D | 81 | 81 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 51 MPa | 7400 psi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Tensile Modulus | 3.1 GPa | 450 ksi | Type 1 - Rigids, 2 in/min; ASTM D638 |
Flexural Modulus | 2.86 GPa | 415 ksi | ASTM D790 |
Flexural Strength | 86.2 MPa | 12500 psi | ASTM D790 |
Izod Impact, Notched | 0.587 J/cm | 1.1 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C | 163 °F | Unannealed, 0.250 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 210 - 216 °C | 410 - 420 °F | Molding |
Descriptive Properties | |
Cell Classification D1784 | 12454 | ASTM D1784 |
NSF | Acceptable | Std 14-Plastic Piping Comp. |
NSF | Acceptable | Std 61-Drinking Water Appl. |
Product Form | Pellets/Cubes | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|