MatWeb, The Online Materials Database

PolyOne Geon® 2199 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • High Impact
  • Transparent
  • High Gloss
  • High Impact at Low Temperature

Applications:

  • FDA (Food Contact)
  • Bottles

Market:

  • Packaging

Processing Method:

  • Blow Molding

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Density0.801 g/cc0.0289 lb/in³ ASTM D1505
Specific Gravity1.31 g/cc0.0473 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D8181 Instantaneous; ASTM D2240
Tensile Strength, Yield42.7 MPa6200 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.21 GPa321 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.39 GPa347 ksi ASTM D790
Flexural Strength75.2 MPa10900 psi ASTM D790

Thermal Properties
Deflection Temperature at 0.46 MPa (66 psi)64.4 °C148 °F Unannealed, 0.125 in bars; ASTM D648

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.