PolyOne Geon® 2540-xx04FRD Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL 75°C
  • Non-migrating, Non-contaminating
  • Mil C-17, 13930 Type JP Coaxial Cable
  • Flame Retardant

Applications:

  • Telecommunication Jacket

Market:

  • Wire & Cable

Processing Method:

  • Extrusion Coating
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.29 g/cc0.0466 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8282 15 sec; ASTM D2240
Tensile Strength, Yield16.5 MPa2400 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break360 %360 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus0.00844 GPa1.224 ksi Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Oxygen Index28 %28 % 0.075 in; ASTM D2863

Processing Properties
Melt Temperature171 - 174 °C340 - 345 °F Extrusion

Descriptive Properties
Immersion - Flexible Strength Change110 % ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543
Immersion - Percent Change of Elongation0 % ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543
Oven Aged - Retention of Elongation (ROE)80 % 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Oven Aged - Retention of Tensile Strength (ROT)95 % 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.