MatWeb, The Online Materials Database
PolyOne Geon® 2540-xx04FRD Vinyl Compound - Wire & Cable
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - UL 75°C
- Non-migrating, Non-contaminating
- Mil C-17, 13930 Type JP Coaxial Cable
- Flame Retardant
Applications: Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.29 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 82 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 2400 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Elongation at Break | 360 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tensile Modulus | 1224 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Thermal Properties |
|
Oxygen Index | 28 % | 0.075 in; ASTM D2863 |
Processing Properties |
|
Melt Temperature | 340 - 345 °F | Extrusion |
Descriptive Properties | |
Immersion - Flexible Strength Change | 110 % | ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543 |
Immersion - Percent Change of Elongation | 0 % | ASTM Oil #2, 250°F (121°C), 18 hrs; ASTM D543 |
Oven Aged - Retention of Elongation (ROE) | 80 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Oven Aged - Retention of Tensile Strength (ROT) | 95 % | 235°F (113°C), 168 hrs (7 days), 0.075 in; UL Standard |
Product Form | Pellets/Cubes | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from