PolyOne Geon® 2710 Amber 9375 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • General Purpose Grade
  • Transparent
  • Amber
  • High Impact
  • High Flow
  • High Gloss
  • UV Stabilized

Applications:

  • General Purpose
  • Hair Care Products
  • Sun Tan Lotions

Processing Method:

  • Injection Blow Molding

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Density52 lb/ft³ ASTM D1505
Specific Gravity1.32 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D80 Instantaneous; ASTM D2240
Tensile Strength, Yield7040 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus366850 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus405 ksi ASTM D790
Flexural Strength12000 psi ASTM D790
Izod Impact, Notched2.2 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
Deflection Temperature at 1.8 MPa (264 psi)67 °F Unannealed, 0.125 in bars; ASTM D648

Optical Properties
Transmission, Visible0 % 30.0 mils, 400 nm
Transmission, Visible39.5 % 30.0 mils, 700 nm

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.