PolyOne Geon® 2710 TRN 9470 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - High Impact
- High Flow
- Transparent
- High Gloss
- UV Stabilized
Applications: - FDA (Food Contact)
- Hotel Amenities
- Mouthwash
- Cosmetics
Processing Method: Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.32 g/cc | 0.0477 lb/in³ | ASTM D792 |
Bulk Density | Max 0.833 g/cc | Max 0.0301 lb/in³ | ASTM D1505 |
Mechanical Properties |
|
Hardness, Shore D | 82 | 82 | Instantaneous; ASTM D2240 |
Tensile Strength, Yield | 44.4 MPa | 6440 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 2.36 GPa | 341.6 ksi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 2.62 GPa | 380 ksi | ASTM D790 |
Flexural Strength | 77.3 MPa | 11210 psi | ASTM D790 |
Izod Impact, Notched | 1.01 J/cm | 1.9 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
Deflection Temperature at 1.8 MPa (264 psi) | 20 °C | 68 °F | Unannealed, 0.125 in bars; ASTM D648 |
Optical Properties |
|
Transmission, Visible | 69 % | 69 % | 30.0 mils, 400 nm |
Transmission, Visible | 85 % | 85 % | 30.0 mils, 700 nm |
Descriptive Properties | |
Product Form | Pellets | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|