PolyOne Geon® 2800 IND-BL-1 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

A high gloss transparent rigid PVC Compound designed for Industrial Blow Molding applications. This Compound is specifically formulated for large clear blow molded parts.

Description/Features:

  • Medium Impact

Applications:

  • General Purpose

Processing Method:

  • Extrusion - Profile, Sheet, Foam, Blow Molding

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Density0.776 g/cc0.028 lb/in³ ASTM D1505
Specific Gravity1.32 g/cc0.0477 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D8282 Instantaneous; ASTM D2240
Tensile Strength, Yield45.5 MPa6600 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break160 %160 % Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.76 GPa401 ksi ASTM D790
Flexural Strength78.6 MPa11400 psi ASTM D790
Izod Impact, Notched7.47 J/cm14 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Processing Properties
Melt Temperature193 - 210 °C380 - 410 °F Blow Molding

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.