PolyOne Geon® 3201-xx05D Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL Recognized per QMFZ2
  • UL 60°C
  • UL 94 HB
  • Flame Retardant

Applications:

  • Apparatus & Cord Molding
  • Plug Molding

Market:

  • Wire & Cable

Processing Method:

  • Molding
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.32 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A62 15 sec; ASTM D2240
Tensile Strength, Yield1800 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break375 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Brittleness Temperature-58 °F ASTM D746
Flammability, UL94HB All Colors; 0.059 in.; PolyOne Internal

Processing Properties
Melt Temperature310 - 320 °F Molding

Descriptive Properties
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.