MatWeb, The Online Materials Database

PolyOne Geon® 3311-xx23D Vinyl Compound - Wire & Cable


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • UL Recognized per QMFZ2
  • UL 75°C
  • Transparent
  • UL 94 V0
  • Flame Retardant

Applications:

  • Apparatus & Cord Molding

Market:

  • Wire & Cable
PolyOne First Choice

Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.33 g/cc ASTM D792

Mechanical Properties
Hardness, Shore D76 15 sec; ASTM D2240
Tensile Strength, Yield7700 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break150 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Flammability, UL94V-0 All Colors; 0.03 in.

Processing Properties
Melt Temperature360 - 380 °F Extrusion

Descriptive Properties
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.