Physical PropertiesMetricEnglishComments
Specific Gravity1.33 g/cc0.048 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A7777 15 sec; ASTM D2240
Tensile Strength, Yield17.7 MPa2560 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break360 %360 % Type 4 - Flexibles, 20 in/min; ASTM D638

Thermal Properties
Brittleness Temperature-30 °C-22 °F ASTM D746
Flammability, UL94V-2V-2 Natural; 0.051 in.
Flammability, UL94V-2V-2 White; 0.051 in.
Flammability, UL94V-0V-0 Black; 0.063 in.
Flammability, UL94V-0V-0 All Colors; 0.11 in.
Oxygen Index28 %28 % 0.075 in; ASTM D2863

Processing Properties
Melt Temperature168 - 174 °C335 - 345 °F Molding

Descriptive Properties
Product FormPellets/Cubes 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.