PolyOne Geon® 6935 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Exterior-Excellent Weatherability
  • High Impact
  • Broad Color Palette
  • UL 94 V0
  • AAMA 303
  • CSA A440

Applications:

  • Custom Profiles
  • Custom Profiles-Thick wall
  • Window Components
  • Fencing Profiles

Market:

  • Windows

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.46 g/cc0.0527 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D7979 15 sec; ASTM D2240
Tensile Strength, Yield41.4 MPa6010 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.99 GPa433.3 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.91 GPa422 ksi ASTM D790
Flexural Strength81.2 MPa11780 psi ASTM D790
Dart Drop Total Energy48.1 J/cm0.09 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy171 J/cm0.32 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched9.98 J/cm18.7 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched11.7 J/cm21.9 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched12.4 J/cm23.3 ft-lb/in Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F64.8 µm/m-°C36 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)72.8 °C163 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0V-0 All Colors; 0.035 in.

Processing Properties
Melt Temperature182 - 193 °C360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178416354 ASTM D1784
Cell Classification D421614143433 ASTM D4216
Ease of SizingExcellent 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.