MatWeb, The Online Materials Database

PolyOne Geon® 78761 Vinyl Compound - Rigid (RPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Interior
  • Chemical Resistant
  • UL 94 V0
  • NSF Type I
  • NSF STD 14
  • NSF STD 61

Applications:

  • Bar & Rod Stock

Processing Method:

  • Extrusion-Single Screw
PolyOne First Choice

Disclaimer: Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.38 g/cc0.0499 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore D8080 15 sec; ASTM D2240
Tensile Strength, Yield50.3 MPa7300 psi Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus2.83 GPa410 ksi Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Modulus2.9 GPa420 ksi ASTM D790
Flexural Strength103 MPa15000 psi ASTM D790
Dart Drop Total Energy64.1 J/cm0.12 ft-lb/mil Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Dart Drop Total Energy144 J/cm0.27 ft-lb/mil Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226
Izod Impact, Notched0.481 J/cm0.9 ft-lb/in Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256
Izod Impact, Notched0.534 J/cm1 ft-lb/in Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256

Thermal Properties
CTE, linear 68°F52.2 µm/m-°C29 µin/in-°F ASTM D696
Deflection Temperature at 1.8 MPa (264 psi)70 °C158 °F Unannealed, 0.125 in bars; ASTM D648
Flammability, UL94V-0V-0 All Colors; 0.75 in.

Processing Properties
Melt Temperature182 - 193 °C360 - 380 °F Extrusion

Descriptive Properties
Cell Classification D178412454 ASTM D1784
Ease of SizingGood 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.