MatWeb, The Online Materials Database
PolyOne Geon® 78812 Vinyl Compound - Flexible (FPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: Applications: Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Information provided by PolyOne Corporation.
Physical Properties | Metric | English | Comments |
|
Specific Gravity | 1.24 g/cc | 0.0448 lb/in³ | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore A | 58 | 58 | 15 sec; ASTM D2240 |
Hardness, Shore A | 63 | 63 | Instantaneous; ASTM D2240 |
Tensile Strength, Ultimate | 11.4 MPa | 1650 psi | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tensile Strength, Ultimate | 4.14 MPa | 600 psi | Type 4 - Flexibles, 2 in/min, 100% in/in; ASTM D638 |
Elongation at Break | 400 % | 400 % | Type 4 - Flexibles, 20 in/min; ASTM D638 |
Tear Strength | 31.6 kN/m | 180 pli | Die C (graves), 20 in/min; ASTM D624 |
Clash Berg Modulus | 0.031 GPa | 4.5 ksi | -31°F (-35°C); ASTM D1043 |
Thermal Properties |
|
Brittleness Temperature | -45 °C | -49 °F | ASTM D746 |
Clash Berg Stiffness Temperature | -45 °C | -49 °F | 45,000 psi; ASTM D1043 |
Processing Properties |
|
Melt Temperature | 168 - 177 °C | 335 - 350 °F | Extrusion |
Descriptive Properties | |
Automotive Approval | DaimlerChrysler, MS-DC225 | |
Product Form | Pellets | |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|