MatWeb, The Online Materials Database

PolyOne Geon® 78815 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Medium Gloss

Applications:

  • General Purpose

Market:

  • Automotive

Processing Method:

  • Extrusion and Molding

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.34 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A86 15 sec; ASTM D2240
Tensile Strength, Ultimate2799 psi 20 in/min; ASTM D638
Elongation at Break290 % 20 in/min; ASTM D638
Tear Strength450 pli Die C (graves), 2 in/min; ASTM D1004

Processing Properties
Melt Temperature360 - 375 °F Extrusion

Descriptive Properties
Automotive ApprovalDaimlerChrysler, MS-DC228 
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.