MatWeb, The Online Materials Database

PolyOne Geon® 82024 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Medium Gloss

Applications:

  • General Purpose

Market:

  • Automotive

Processing Method:

  • Extrusion and Molding

Disclaimer: Note: Automotive OEM approval(s).

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.2 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A46 15 sec; ASTM D2240
Hardness, Shore A52 Instantaneous; ASTM D2240
Tensile Strength, Ultimate1100 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Strength, Ultimate300 psi Type 4 - Flexibles, 2 in/min, 100% in/in; ASTM D638
Elongation at Break450 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength110 pli Die C (graves), 20 in/min; ASTM D624
Clash Berg Modulus2000 psi -31°F (-35°C); ASTM D1043

Thermal Properties
Brittleness Temperature-76 °F ASTM D746
Clash Berg Stiffness Temperature-67 °F 45,000 psi; ASTM D1043

Processing Properties
Melt Temperature320 - 335 °F Extrusion

Descriptive Properties
Automotive ApprovalDaimlerChrysler, MS-DC225 
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.