PolyOne Geon® 85885 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior-Weatherable Dark Browns
- AAMA 303
Applications: - Window Components
- Custom Profiles
Market: Processing Method: PolyOne First ChoiceDisclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
Physical Properties | Original Value | Comments |
|
Specific Gravity | 1.35 g/cc | ASTM D792 |
Mechanical Properties |
|
Hardness, Shore D | 83.2 | 15 sec; ASTM D2240 |
Tensile Strength, Yield | 8320 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Tensile Modulus | 427600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
Flexural Modulus | 443 ksi | ASTM D790 |
Flexural Strength | 13720 psi | ASTM D790 |
Dart Drop Total Energy | 0.1 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Dart Drop Total Energy | 0.32 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
Izod Impact, Notched | 1.3 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 1.6 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Izod Impact, Notched | 1.7 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
CTE, linear 68°F | 38 µin/in-°F | ASTM D696 |
Deflection Temperature at 1.8 MPa (264 psi) | 156 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
Melt Temperature | 360 - 380 °F | Extrusion |
Descriptive Properties | |
Cell Classification D1784 | 13553 | ASTM D1784 |
Cell Classification D4216 | 12145423 | ASTM D4216 |
|
|
|
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
|