MatWeb, The Online Materials Database
PolyOne Geon® 85889 Vinyl Compound - Rigid (RPVC)
Subcategory: Polymer; Thermoplastic; Vinyl
Material Notes:
Description/Features: - Exterior-Weatherable
- High Flow
- High Gloss
Applications: - Custom Profiles
- Greenhouse Trim
Market: Processing Method: Disclaimer: Note: Automotive OEM approval(s). Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
| Physical Properties | Original Value | Comments |
|
| Specific Gravity | 1.36 g/cc | ASTM D792 |
Mechanical Properties |
|
| Hardness, Shore D | 81.9 | 15 sec; ASTM D2240 |
| Tensile Strength, Yield | 6470 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Tensile Modulus | 362600 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
| Flexural Modulus | 369 ksi | ASTM D790 |
| Flexural Strength | 10860 psi | ASTM D790 |
| Dart Drop Total Energy | 0.13 ft-lb/mil | Procedure A, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Dart Drop Total Energy | 0.29 ft-lb/mil | Procedure B, 0.125 in Conical Dart, 73°F (23°C); ASTM D4226 |
| Izod Impact, Notched | 16 ft-lb/in | Method A, Injection Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 4.2 ft-lb/in | Method A, With Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
| Izod Impact, Notched | 8.7 ft-lb/in | Method A, Against Grain - Comp. Molded, 0.125 in bars, 73°F (23°C); ASTM D256 |
Thermal Properties |
|
| CTE, linear 68°F | 46 µin/in-°F | ASTM D696 |
| Deflection Temperature at 1.8 MPa (264 psi) | 163 °F | Unannealed, 0.125 in bars; ASTM D648 |
Processing Properties |
|
| Melt Temperature | 360 - 380 °F | |
Descriptive Properties | |
| Automotive Approval | General Motors, GMP 7001M PVC | |
| Cell Classification D1784 | 16344 | ASTM D1784 |
| Cell Classification D4216 | 14243233 | ASTM D4216 |
| Ease of Sizing | Acceptable | |
|
|
 |
Copyright 1996-2010 by Automation Creations, Inc. The information provided by
MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not
be reproduced either electronically, photographically or substantively without permission from
Automation Creations, Inc. No warranty, neither expressed nor implied, is given
regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of
information from MatWeb.
|
 |