Disclaimer: NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is “For foods of high water content only”. This material is also listed under NSF Std. 61. This listing covers many uses and restrictions may apply depending on the application. It is the customer's responsibility to ensure that the compound is suitable for its intended application. Please contact us to review the suitability of specific products in specific applications.

Information provided by PolyOne Corporation.

Physical PropertiesMetricEnglishComments
Specific Gravity1.24 g/cc0.0448 lb/in³ ASTM D792

Mechanical Properties
Hardness, Shore A8484 15 sec; ASTM D2240
Hardness, Shore A9090 Instantaneous; ASTM D2240
Tensile Strength, Ultimate10.7 MPa1550 psi Type 4 - Flexibles, 20 in/min, 100% in/in; ASTM D638
Tensile Strength, Ultimate18.3 MPa2650 psi Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break400 %400 % Type 4 - Flexibles, 20 in/min; ASTM D638
Tear Strength76.3 kN/m435 pli Die C (graves), 20 in/min; ASTM D624

Thermal Properties
Brittleness Temperature-27 °C-16.6 °F ASTM D746

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.