MatWeb, The Online Materials Database

PolyOne Geon® 86509 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

Description/Features:

  • Low Migration
  • Low taste and odor

Applications:

  • Gaskets - Refrigerator

Market:

  • Appliance

Processing Method:

  • Extrusion

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.45 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A66 15 sec; ASTM D2240
Hardness, Shore A74 Instantaneous; ASTM D2240
Tensile Strength, Ultimate1700 psi 20 in/min; ASTM D638
Elongation at Break350 % 20 in/min; ASTM D638
Tear Strength230 pli Die C (graves), 20 in/min; ASTM D624

Processing Properties
Melt Temperature345 - 355 °F Extrusion

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.