MatWeb, The Online Materials Database

PolyOne Geon® 86851 Vinyl Compound - Flexible (FPVC)


Subcategory: Polymer; Thermoplastic; Vinyl

Material Notes:

General Purpose Clear PVC Compound with low level of UV inhibitor.

Description/Features:

  • Transparent

Applications:

  • Floor Mats
  • General Purpose
  • Hose and Tubing

Processing Method:

  • Extrusion and Molding
  • Extrusion-Sheet

Information provided by PolyOne Corporation.

Physical PropertiesOriginal ValueComments
Specific Gravity1.21 g/cc ASTM D792

Mechanical Properties
Hardness, Shore A79 15 sec; ASTM D2240
Hardness, Shore A85 Instantaneous; ASTM D2240
Tensile Strength, Ultimate1200 psi 20 in/min, 100% in/in; ASTM D638
Tensile Strength, Ultimate2400 psi 20 in/min; ASTM D638
Elongation at Break420 % 20 in/min; ASTM D638
Tear Strength420 pli Die C (graves), 20 in/min; ASTM D624

Thermal Properties
Brittleness Temperature-27 °F ASTM D746

Processing Properties
Melt Temperature345 - 355 °F Extrusion
Melt Temperature380 - 400 °F Molding

Descriptive Properties
Product FormPellets 

 


Copyright 1996-2010 by Automation Creations, Inc.  The information provided by MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from Automation Creations, Inc. No warranty, neither expressed nor implied, is given regarding the accuracy of this information. The user assumes all risk and liability in connection with the use of information from MatWeb.